Dear colleagues,

Currently I'm thinking to make a mold for some high
aspect-of-ratio columns (about 20 micron high with
diameter of 5 micron). Originally I want to use some
dry-etch BCB, but unfortunately find it very expensive
(US $3250 for 0.9 Kg). Anyone can suggest some
alternatives? Thanks a lot.

Best regards,

Ebin

__________________________________
Do you Yahoo!?
Protect your identity with Yahoo! Mail AddressGuard
http://antispam.yahoo.com/whatsnewfree

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
University Wafer
MEMStaff Inc.