PAtrick Carlberg
wet etchant for Sn and Sn oxide
2003-11-06
Robert Dean
2003-11-07
rakesh babu
2003-11-07
Mighty Platypus
2003-11-07
David Nemeth
wet etchant for Sn and Sn oxide
David Nemeth
2003-11-07
It should be added that Hydrobromic acid is pretty nasty stuff - talk to
your facilities people before you even order it.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On
Behalf Of rakesh babu
Sent: Thursday, November 06, 2003 10:07 PM
To: General MEMS discussion
Subject: Re: [mems-talk] wet etchant for Sn and Sn oxide


dear sir,

 Tin and Tin oxide are difficult to etch using wet etchant and the only wet
etchant found to etch it is Hydrobromic acid.

best regards
Rakesh
Graduate Research Assistant
ECE  Department
Wayne state University

Robert Dean  wrote:
Hello,

Can someone recommend a wet etchant for Sn and Sn oxide that does not etch
Si, Ni or Ti?

Thanks!

Sincerely,

Robert Dean

Research Associate IV
Center for Advanced Vehicle Electronics
Auburn University
200 Broun Hall
Auburn, AL 36849

Voice: 334-844-1838
Fax: 334-844-1898
Email: [email protected]
Web: http://www.eng.auburn.edu/~deanron


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

---------------------------------
Do you Yahoo!?
Protect your identity with Yahoo! Mail AddressGuard
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Addison Engineering