A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Protective Coating in KOH solution!!!!
Protective Coating in KOH solution!!!!
2003-11-07
KANISHKA BISWAS
RE : [mems-talk] Protective Coating in KOH solution!!!!
2003-11-07
Christophe Gorecki
2003-11-07
Shane Jones
2003-11-07
Zhang, Wenyue(Lydia)
2003-11-12
Neal Ricks
2003-11-14
Glenn Silveira
2003-11-07
Michael L
2003-11-14
Kretschmer Hans-Richard
Protective Coating in KOH solution!!!!
Glenn Silveira
2003-11-14
Depending on the need for post etch removal, there are a couple of
dielectric PECVD films ie. Si3N4 and (a)SiC  that will hold up to your wet
etch process

P.S. I can deposit both of these films if you need them.

Best regards,

Glenn Silveira


EIF Division

KANISHKA BISWAS  wrote:
Hi Everybody,
Can any one suggest a protective coating (polymer etc)for protecting the top
surface of silicon wafer with aluminium lines while etching the back side of
the wafer using KOH solution???? We have already tried out wax, black wax
coatings but it did not work.
Any help and references in this regard will be highly appreciated....
Thanks
Kanishka


____________________________________________________________



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Tanner EDA by Mentor Graphics
MEMS Technology Review