MEMSnet Home: MEMS-Talk: metal? etch mask for TMAH
metal? etch mask for TMAH
2003-10-29
Karin Buchholz
2003-10-30
Shile
2003-11-18
Martyna
2003-11-18
Massimiliano Decarli
2003-11-19
David Nemeth
SiO2 sputtering rate
2003-11-21
Oray Orkun Cellek
In search for another room-temp casting material on silicon
2003-11-18
Wei-han J. Wu
metal? etch mask for TMAH
Massimiliano Decarli
2003-11-18
Hy Martina,
Your problem is that gold/silicon combination forms a galvanic cell.
In fact this tecnique is already used and it is called galvanic etch stop.
Here you can find more on this topic:
http://www.dimes.tudelft.nl/1998/s2/c2/c2-1-fundamentals.html

Max


From: "Martyna" 
To: 
Sent: Tuesday, November 18, 2003 11:50 AM
Subject: ITCSpam: [mems-talk] metal? etch mask for TMAH


> Hello,
>
> Does anybody know if gold mask can be used for TMAH etching? I have 1000 A
gold layer (with 100 A Cr) on a Si wafer. I used 5% TMAH and etch for half
an hour. The result is much below the typical etch rate.
>
> Before etching I removed native oxide with HF.
>
> Thank you for your help
>
> Martyna
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Nano-Master, Inc.
MEMS Technology Review