The Young's modulus E is a material property. This constant correlates the
applied stress to the corresponding strain on a given material using Hooks law.
This constant is defined only for elastic deformation of materials at which the
deformation on materials is reversible and the deformation disappears when the
applied stress is removed. Young's modulus=Stress/Strain. The constant E is the
slope of elastic portion on of stress-strain curve of a given material, then it
depends on material type. This is what we refer to as Young's (Elastic) modulus
of materials.
In Micro-scale and Nano-scale components, the response of materials changes
dramatically. However, the definition of Young's modulus stay the same
regardless of quantity of this constant as it is compared with macro-sized
components.
Thanks,
Ahmad

----- Original Message -----
From: Jackle D 
Date: Thursday, November 20, 2003 8:53 am
Subject: [mems-talk] what decide the value of Young's modulus

> Dear all:
>
> I want to do some research-work about Young's modulus of
> thin/thick films, would you kindly tell me Young's modulus is
> related to what? What makes material a big, or low Young's
> modulus?
> Any advice is appreciated.
>
> Regards!
>
> jackle
>
>
>
>
> ---------------------------------
> Do you Yahoo!?
> Free Pop-Up Blocker - Get it now
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-
> talkHosted by the MEMS Exchange, providers of MEMS processing
> services.Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation