Steven F. Nagle
2003-11-21
I imagine you've tried ferric choloride, but Transene should have a
quality mix:
    http://www.transene.com/cu_etchant.html

If not, one of their engineers could point you in the right direction.
-Steven


Werner Karl wrote:

>Dear All,
>
>     I am looking for a good copper wet-etchant, that allows the controlled
>and uniform etching of fine structures.
>     The "standard" solutions I have tried so far, all etch either very
>rapidly, resulting in large undercut, or non-uniform. Thanks for your help,
>
>Werner.
>
>Werner J. Karl
>Imperial College, London
>[email protected]
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Harrick Plasma, Inc.
Addison Engineering