quartz furnace tube
2003-11-20
Yuanfang Gao
2003-11-21
Julie Houser
2003-11-21
R. Brent Garber (2 parts)
quartz furnace tube
R. Brent Garber
2003-11-21
Yuanfang,

I have always made my own.  You order the glass tube and have a glass shop cut
it to size and shape.
I have them close one end down to a 3/8 tube for gas or steam to enter.  I have
bought glass vessel and had then reshaped to make end caps.  The University of
Connecticut has its own glass shop that did all the work.  Try look for the
technical service department on
the UCONN.edu web site for the glass shop.

Brent

Yuanfang Gao wrote:

> Dear all,
>
> I am going to build up a furnace system using the Lindberg tube furnace. Could
anyone suggest a good supplier for quartz processing tubes and the accessories
such as the end caps, wafer boats, rods etc? I hope I can run gas through the
tubes. Thank you very much!
>
> Yuanfang Gao
> ECE Dept.
> U. of Missouri-Columbia
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
garber.vcf (text/x-vcard, 361 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.