SiO2 sputtering rate
2003-11-21
[email protected]
SiO2 sputtering rate
[email protected]
2003-11-21
I would definately reduce pressure to the range you are talking about but I
would also increase the power level to around 500 watts if you have the
capability. Everything else looks fine as far as I can see. bob Henderson

reply