Hi,
        I need to fabricate IDE's with pitch of 3 um . the metal layer on the
IDE is 2 um.I am using Cu as the top electrode.
      Does anybody have any experience with etching/ lift off of Cu in IDE
fabrication.Any information, process conditions etc will be highly appreciated.
        Thanks in advance,
                  Dipankar


____________________________________________________________
Get advanced SPAM filtering on Webmail or POP Mail ... Get Lycos Mail!
http://login.mail.lycos.com/r/referral?aid=27005

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
MEMStaff Inc.