MEMSnet Home: MEMS-Talk: Brown LPCVD Polysilicon
Brown LPCVD Polysilicon
2003-11-25
bob barker
2003-11-26
Tim Watson
Brown LPCVD Polysilicon
bob barker
2003-11-25
Can anyone tell me why my LPCVD polysilicon is brown and/or black?  I am
depositing it at 620 C and 300 mTorr with a flow rate of 50 sccm of silane.  The
inside of the quartz furnace tube is coated with silicon, so I'm not sure the
temperature inside the tube is really 620 C.  Do I need to clean it?  If so, how
do I do that?

Thanks,

Robert Barker





---------------------------------
Do you Yahoo!?
Free Pop-Up Blocker - Get it now
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics