MEMSnet Home: MEMS-Talk: Diamond
Simple Young's Modulus for Silicon... Please
2003-11-25
Pete Crompton
2003-11-26
Imran Ghauri
Diamond
2003-11-26
VIKAS
2003-11-26
Imran Ghauri
2003-11-26
RobDavis
2003-11-28
Jim Intrater
2003-12-01
David Nemeth
2003-11-26
Yilei Zhang
Diamond
Jim Intrater
2003-11-28
What are you presently using?

-JI
----- Original Message -----
From: "VIKAS" 
To: "General MEMS discussion" 
Sent: Wednesday, November 26, 2003 7:42 AM
Subject: [mems-talk] Diamond


>
> Hi,
> Can anyone give me some information about the feasibility of diamond as a
> bearing material, particularly the cost of fabrication etc. Any good links
> would be helpful.
> Thank you
>
> Vikas
> Senior Undergraduate,
> Mechanical Engineering Dept.
> IIT Bombay.
>
>
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
University Wafer
Tanner EDA by Mentor Graphics