MEMSnet Home: MEMS-Talk: Looking for information on low temperature glass-frit sealingprocess
Looking for information on low temperature glass-frit sealing process
2003-11-30
Huxiaodong
Looking for information on low temperature glass-frit sealingprocess
2003-12-01
Paolo Bondavalli
Looking for information on low temperature glass-frit sealingprocess
Paolo Bondavalli
2003-12-01
Dear Hu,
It is not possible to reach less than 390°C.
If it was possible, everybody could use it!
Bye


Huxiaodong a écrit :

> Dear MEMS Community,
> Does anyone know about any glass-frit bonding process for WLP package of MEMS
devices that has a process temperature below 300 Celcuis degree?
> Any information will be greatly appreciated.
> Yours Sincerely,
> Hu Xiaodong.
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

--
*********************************************************
Dr. Paolo Bondavalli
R&D MEMS Engineer
MICROTEC MEMS
THALES (ex THOMSON-CSF) CORPORATE RESEARCH CENTER
Domaine de Corbeville,
Route Departementale 128
F91404 ORSAY
(FRANCE)
Tel : 01 69 33 08 63
Fax : 01 69 33 08 62
Email : [email protected]
**********************************************************
Disclaimer: Opinions expressed herein are my own and may
  not represent those of my employer.
**********************************************************



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
The Branford Group
Addison Engineering