A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Lift-Off
Lift-Off
2003-12-03
Krueger, Bernd (Unaxis Optics BZ)
2003-12-04
Jim Beall
2003-12-04
Shane Jones
2003-12-04
Neal Ricks
2003-12-05
ShuTing Hsu
2003-12-05
Karin Buchholz
2003-12-05
William Lanford-Crick
2003-12-04
Michael D Martin
Lift-Off
Neal Ricks
2003-12-04
Hello Bernd,
Shipley Co. offers standard products for such a Lift-Off process.  There is a
two coat system, with one developer solution used.  The two resist products I
use are called LOL2000, and Microposit 1813, but the key is the LOL2000.  The
pattern is Developed using a third product, LDD-26W.

Regards,
Neal


"Krueger, Bernd (Unaxis Optics BZ)"  wrote:
Dear All,

does anybody has experience in a metal-lift-off-process? I am searching for
a resist working fine for soft metal with a thickness of about 300nm. May be
you can advise me either negative or positive resists.

I would appreciate any help,
Thanks in advance,

Bernd Krueger


> Manager Engineering, OPO
> mailto:[email protected]
>
> Unaxis Balzers Ltd.
> Division Optics
> P.O. Box 1000
> FL-9496 Balzers / Liechtenstein
> Tel. +423 / 388 4932
> Fax. +423 / 388 5185
>
> Unaxis Optics -
> the future of Balzers Thin Films
>
> http://www.optics.unaxis.com
>



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

---------------------------------
Do you Yahoo!?
Free Pop-Up Blocker - Get it now
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group