A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Lift-Off
Lift-Off
2003-12-03
Krueger, Bernd (Unaxis Optics BZ)
2003-12-04
Jim Beall
2003-12-04
Shane Jones
2003-12-04
Neal Ricks
2003-12-05
ShuTing Hsu
2003-12-05
Karin Buchholz
2003-12-05
William Lanford-Crick
2003-12-04
Michael D Martin
Lift-Off
Karin Buchholz
2003-12-05
Hi Bernd,

we use the Microposit S1818 for Lift-off, it is quite thick (the last
two numbers are related to the thickness, so the S1805 is much thinner
at the same spin rate) p.e.the S1818 is arond 1.6 µm @ 6000 rpm, 40s. To
get an undercut you can also try to put the samples 15 min in
Chlorobenzene after the softbake and exposure before the development.
(Chlorobenzene is tumourigenic, so use a well ventilated place and
prevent Daylight exposure during the 15 min, p.e. by aluminum Foil)

Good luck,

Karin


Krueger, Bernd (Unaxis Optics BZ) schrieb:

>Dear All,
>
>does anybody has experience in a metal-lift-off-process? I am searching for
>a resist working fine for soft metal with a thickness of about 300nm. May be
>you can advise me either negative or positive resists.
>
>I would appreciate any help,
>Thanks in advance,
>
>Bernd Krueger
>

--
Dipl.-Ing. Karin Buchholz

Walter Schottky Institut
Technische Universitaet Muenchen
email: [email protected]





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering