A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Lift-Off
Lift-Off
2003-12-03
Krueger, Bernd (Unaxis Optics BZ)
2003-12-04
Jim Beall
2003-12-04
Shane Jones
2003-12-04
Neal Ricks
2003-12-05
ShuTing Hsu
2003-12-05
Karin Buchholz
2003-12-05
William Lanford-Crick
2003-12-04
Michael D Martin
Lift-Off
William Lanford-Crick
2003-12-05
We use 1813 on top of LOR-B for metal liftoff as well as AZ-5214 with image
reversal.  Both processes give a nice undercut profile for lift-off.  If
either of these are options for you, I can give you specific processes.

AZ-5214 is nice to have around because it can be used either as a positive
or a negative-tone resist.

BTW, also  make sure that metal evaporation is normal to your substrate,
i.e. the sample is placed directly over the metal source in evaporator or
sputterer.  This will help ensure clean lift-off because the resist
side-walls are less likely to have metal on them.

-Bill Lanford-Crick

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of
Karin Buchholz
Sent: Friday, December 05, 2003 1:40 AM
To: General MEMS discussion
Subject: Re: [mems-talk] Lift-Off


Hi Bernd,

we use the Microposit S1818 for Lift-off, it is quite thick (the last
two numbers are related to the thickness, so the S1805 is much thinner
at the same spin rate) p.e.the S1818 is arond 1.6 µm @ 6000 rpm, 40s. To
get an undercut you can also try to put the samples 15 min in
Chlorobenzene after the softbake and exposure before the development.
(Chlorobenzene is tumourigenic, so use a well ventilated place and
prevent Daylight exposure during the 15 min, p.e. by aluminum Foil)

Good luck,

Karin


Krueger, Bernd (Unaxis Optics BZ) schrieb:

>Dear All,
>
>does anybody has experience in a metal-lift-off-process? I am searching for
>a resist working fine for soft metal with a thickness of about 300nm. May
be
>you can advise me either negative or positive resists.
>
>I would appreciate any help,
>Thanks in advance,
>
>Bernd Krueger
>

--
Dipl.-Ing. Karin Buchholz

Walter Schottky Institut
Technische Universitaet Muenchen
email: [email protected]




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
MEMS Technology Review
Addison Engineering