fluorocarbon residue removal in silicon DRIE
2003-12-05
roberto Campedelli
2003-12-05
Debjyoti Banerjee, Ph.D.
2003-12-08
Sunil Kumar
fluorocarbon residue removal in silicon DRIE
Sunil Kumar
2003-12-08
Fluorocarbon like C4F8 can be removed after a DRIE run by doing a 10-15 minute
piranha etch (5:1 98% H2SO4: 30% H2O2)
you can also try ammonium persulphate instead of H2O2, since its an exothermic
reaction, there is no need to heat the solution

-Sunil

  ----- Original Message -----
  From: roberto Campedelli
  To: [email protected]
  Cc: [email protected]
  Sent: Friday, December 05, 2003 2:28 PM
  Subject: [mems-talk] fluorocarbon residue removal in silicon DRIE


  Hello, did you solve the problem with removing fluorocarbon polymers?

  Roberto Campedelli
  process engineer STMicroelectronics

  _______________________________________________
  [email protected] mailing list: to unsubscribe or change your list
  options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
  Hosted by the MEMS Exchange, providers of MEMS processing services.
  Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
MEMS Technology Review