Etch mask for glass etching
Wong
2003-12-09
i didn't try the evaporation method before but the best result will be using
another masking layer with a optimizing condition... 4 times better than using
the cr/au ...

________________________________

From: [email protected] on behalf of
Aegis
Sent: Sun 12/7/2003 2:36 PM
To: 'General MEMS discussion'
Subject: RE: [mems-talk] Etch mask for glass etching



I do not understand the exactly meaning of "collapse and give way to". If
you mean the Cr/Au film swinging in etchant just like tissues in water (but
no separate from glass), I can tell you the same thing happened in the DC
sputtering film (Cr/Au:400A/1500A). The serious problem of sputtering film
is pinhole in the HF etching process, although additional PR layer will
help.
May I ask the pinholes also happened by using resistive evaporation method?


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Tom Fan
Sent: Saturday, December 06, 2003 9:28 AM
To: [email protected]
Subject: [mems-talk] Etch mask for glass etching

Hi All,

When people use Cr/Au as the etch mask for wet etching of glass, what kind
of
deposition method did they use? I used resistive evaporation method and
found
the metal film collapsed and gave way to the etchant in a very short time. I

suspect the film adhesion is not that good. Maybe sputtering will do a
better
job? Anybody had experience with this situation? Any thoughtful input would
be
appreciated.

Thanks,
Tom Fan

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Addison Engineering
MEMS Technology Review