MEMSnet Home: MEMS-Talk: SU-8 50 wrinkling issue
SU-8 50 wrinkling issue
2003-12-12
[email protected]
2003-12-15
Michael L
2003-12-15
Brubaker Chad
2003-12-15
[email protected]
2003-12-23
[email protected]
2003-12-23
Mighty Platypus
Re: SU-8 50 wrinkling issue
2003-12-25
[email protected]
SU-8 50 wrinkling issue
[email protected]
2003-12-12
Dear all,
i am using SU-8 25 to fabricate a 27 micron feature on a 3 inch
glass wafer (Ti seed layer).After the completion of this process, i am
fabricating a 200 microns thick channel as a second layer using SU-8
50.The process parameters for the 200 microns are the following:
200 process parameters (7ml SU-8 50)

?
Spin: 500rpm for 10sec (100rpm/s ramp)
    1500rpm for 30 sec (300rpm/s ramp)
i.e 500.100.10 and 1500.300.30

?
Leave for 1 min

?
Prebake : 65C for 6 minutes and 95C for 22 minutes
?
Exposure: 160microJ/cm2
?
Postbake: 2min at 65C and 95C for 7 minutes
?
Development: 8-10 min with EC Solvent, Clean with IPA afterwards

The problem is that during the prebake phase,the su-8 wrinkles
irreversibly.as a result the structures are very rough
I would very much appreciate any help and/or recommendations on this
problem.Thank you in advance for your help.I am looking forward to your
reply.


________________________________________________________________

DISCLAIMER:

This e-mail and any files transmitted with it are confidential
and intended solely for the use of the individual or entity to
whom it is addressed.  If you are not the intended recipient
you are prohibited from using any of the information contained
in this e-mail.  In such a case, please destroy all copies in
your possession and notify the sender by reply e-mail.  Heriot
Watt University does not accept liability or responsibility
for changes made to this e-mail after it was sent, or for
viruses transmitted through this e-mail.  Opinions, comments,
conclusions and other information in this e-mail that do not
relate to the official business of Heriot Watt University are
not endorsed by it.
________________________________________________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing