MEMSnet Home: MEMS-Talk: Hydrophilic PDMS
Hydrophilic PDMS
2003-12-11
Benoit Ladoux
2003-12-11
Bill Moffat
2003-12-15
Michael D Martin
Hydrophilic PDMS
Michael D Martin
2003-12-15
I think that if you use this technique you've got to be careful ... the contact
angle/ surface tension using a plasma treatment only is likely to change as a
function of time.
-Mike

>>> [email protected] 12/11/03 11:55 AM >>>
Benoit,
       Any plasma gas will cause a change in surface tension.  This means you
can use an inert gas such as Argon, change the surface but not actively eat the
PDMS.  Bill Moffat

-----Original Message-----
From: Benoit Ladoux [mailto:[email protected]]
Sent: Thursday, December 11, 2003 8:23 AM
To: [email protected]
Subject: [mems-talk] Hydrophilic PDMS


Dear colleagues,
Besides using oxygen plasma treat PDMS surface, are there any other ways to
change it from hydrophobic into hydrophilic?
Sincerely yours
Benoit Ladoux


--------------------------------------------------------------------------------
-----------------
Benoit Ladoux
LBHP-Université Paris 7
Case 7056, Tour 33-34/2ème étage, 2 place Jussieu
75251 Paris cedex 05
Tel:+33 (0)1 44 27 61 10 ; Fax:+33 (0)1 44 27 43 35
--------------------------------------------------------------------------------
-----------------
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
MEMStaff Inc.
The Branford Group