How to make the membrane flat?
Neal Ricks
2003-12-15
You could try e-beam deposition of a highly tensile film to flatten it out.
Perhaps the patterning of a 0.2 micron Nickel film, for example.





miaomin  wrote:
Hi£¬Colleagues
I have made some membrane bridge suspended by 4 springs,which is made of heavy
boron doped layer for KOH stop.The bridge is about 2.5 ~4 micron thick. However,
I found it distorted by the large intrinsic stress (or stress gradient)from
heavy doping. Can anyone give me some advice on how to make the membrane bridge
as flat as it is designed,and yet the temperature is kept under 400degree.Thx in
advance.



¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡ÖÂ
Àñ£¡


¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡miaomin
from IME,Peking Univ. China
¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡[email protected]
¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡¡2005-12-12



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

---------------------------------
Do you Yahoo!?
Protect your identity with Yahoo! Mail AddressGuard
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
University Wafer