MEMSnet Home: MEMS-Talk: Photoresist or Cr delamination problem
Photoresist or Cr delamination problem
2003-12-18
Richard Beaudry
Photoresist or Cr delamination problem
Richard Beaudry
2003-12-18
Hi Pimpim,

I had some adhesion problem before. I solve my problem by first
pre-cleanning the samples just before loading them in the E-beam with
HCl(5%)  and then HF(5%). And then after the lift-off and photoresist
stripping I have done a Rapid Thermal Annealling of 60 sec at 350C.

The metal I use is Cr/Ni/Au   with 10nm/25nm/250 nm

Good luck

Richard Beaudry
Associé de recherche
Laboratoire de micro-fabrication
École Polytechnique



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
Harrick Plasma, Inc.
University Wafer