Jason Viotty
2003-12-23
The adhesion of Pt on the materials you mention is normally quite poor. An
adhesion-layer is normally used (e.g. CT, Ti, Pt).
We have sputtered Pt directly onto low-stress nitride in the past and the
adhesion there was fine (tested with scotch-test). Some people also make
Pt-silicide by depositing Pt directly on Si and then doing an anneal-step,
but I don't know if they take additional precautions to get proper adhesion
of the Pt on the Si.
Succes.

Jason

___________________________________________________________
Jason Viotty
Senior Process Engineer
C2V
http://www.c2v.nl


-----Original Message-----
From: Raj Kumar [mailto:[email protected]]
Sent: zaterdag 20 december 2003 5:51
To: [email protected]
Subject: [mems-talk] Adhesion of Pt on Si, SiO2 and Si3N4



Hello Memsnetigens

     Can anybody tell me adhesion behaviour of sputtered and e-beam
evaporated Platinum layer on Si, Si3N4 and SiO2.

 RAJKUMAR
 SCL,INDIA
____________________________________________________________________________
_






_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Tanner EDA by Mentor Graphics
MEMStaff Inc.