A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: cleaning small chips
cleaning small chips
2003-12-20
Jen Robertson
2003-12-22
Vonda C Alexander
2003-12-22
Steven F. Nagle
2003-12-23
Absara Micro Systems
YBCO contamination?
2004-01-08
Oray Orkun Cellek
2003-12-25
Jack Mulligan
2003-12-21
Phillipe Tabada
2003-12-21
Phillipe Tabada
2003-12-23
Jason Viotty
2003-12-23
Bill Moffat
cleaning small chips
Jason Viotty
2003-12-23
We have had the same problem in the past. We've tried different solvents and
solutions (e.g. Acetone, IPA, RCA), but none of these seemed to help. Also
an oxygen-plasma clean did not give the desired result. The problem seems to
sit  in the fact that the residu seems to be a mixture of organic-residue
and silicon-particles. We eventually solved the problem by putting the chips
for a couple of minutes in a KOH-solution (approx. 25wt%) at aproximately
60?C. The wafers were then gently rinsed in DI-water, followed by and
IPA-rinse (which facilitates drying).
Of course, the usage of a KOH-solution is only possible if your devices do
not have any exposed silicon, or other layers that are not KOH-resistant
(e.g. Al, Ti).
Succes.

Jason

___________________________________________________________
Jason Viotty
Senior Process Engineer
C2V
http://www.c2v.nl


-----Original Message-----
From: Jen Robertson [mailto:[email protected]]
Sent: zaterdag 20 december 2003 2:05
To: [email protected]
Subject: [mems-talk] cleaning small chips


Hi-

Is there a good way to clean small (<5mm square) silicon chips? Our chips
have lots of visiable residues after the dicing process, either from the
dicing tapes or wafer dusts. We have tried soaking in many different
solvents but cannot seem to get rid of them. These chips have fragile MEMS
structures on them and will break if we use ultrasonic agitation. Any
suggestion would be greatly appreciated. Thanks!


Jen


---------------------------------
Do you Yahoo!?
Free Pop-Up Blocker - Get it now
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
MEMS Technology Review
Addison Engineering