A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: cleaning small chips
cleaning small chips
2003-12-20
Jen Robertson
2003-12-22
Vonda C Alexander
2003-12-22
Steven F. Nagle
2003-12-23
Absara Micro Systems
YBCO contamination?
2004-01-08
Oray Orkun Cellek
2003-12-25
Jack Mulligan
2003-12-21
Phillipe Tabada
2003-12-21
Phillipe Tabada
2003-12-23
Jason Viotty
2003-12-23
Bill Moffat
cleaning small chips
Bill Moffat
2003-12-23
Jen,
    One of our customers asked for a special plasma cleaner to handle chips in a
waffle pack to help with this problem.  Contact me directly and I will go into
greater detail.  Bill Moffat

-----Original Message-----
From: Jen Robertson [mailto:[email protected]]
Sent: Friday, December 19, 2003 5:05 PM
To: [email protected]
Subject: [mems-talk] cleaning small chips


Hi-

Is there a good way to clean small (<5mm square) silicon chips? Our chips have
lots of visiable residues after the dicing process, either from the dicing tapes
or wafer dusts. We have tried soaking in many different solvents but cannot seem
to get rid of them. These chips have fragile MEMS structures on them and will
break if we use ultrasonic agitation. Any suggestion would be greatly
appreciated. Thanks!


Jen


---------------------------------
Do you Yahoo!?
Free Pop-Up Blocker - Get it now
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
The Branford Group
Harrick Plasma, Inc.