How to remove edge bead of negative resist
2003-12-23
Yuzhu Li
2003-12-24
Shay Kaplan
How to remove edge bead of negative resist
Shay Kaplan
2003-12-24
after the spin cycle has completed, inject solvent from the bottom in
direction of the rim while spinning the wafer at ~400-500RPM. then spin few
seconds at ~3000RPM for drying
Shay

Yuzhu Li wrote:

> I have been using "cover-expose-develop" method to remove edge bead of
> positive resist. I had to use aceton Q-tip to srub negative eadge bead, is
> there a better way?
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMStaff Inc.