A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: help
AZ5214 remover
2003-12-30
Nadav Agian
2003-12-30
Jack Mulligan
2003-12-30
David Schreiber
2003-12-30
[email protected]
2004-01-05
Jason Viotty
help
2004-01-05
[email protected]
2004-01-05
T. Hamano
help
[email protected]
2004-01-05
hello all
pls any one suggest me the post bake temperature before HF etching photoresist
i used SR 1813.
regards
rajan malik


Quoting Jason Viotty :

> If your devices are not fragile, you could try doing an ultrasonic
> cleaning
> in Acetone. We often use this method to remove toughened resist.
>
> ___________________________________________________________
> Jason Viotty
> Senior Process Engineer
> C2V
> http://www.c2v.nl
> ___________________________________________________________
>
>
> -----Original Message-----
> From: Nadav Agian [mailto:[email protected]]
> Sent: dinsdag 30 december 2003 12:38
> To: [email protected]
> Subject: [mems-talk] AZ5214 remover
>
>
> I am using an AZ5214 P.R as a protective coating for dicing .
> I tried to remove the coating with Acetone , but I still have some
> residuals
> around the Al lines.
> Is there a better way to remove those marks ?
>
>
> Nadav
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



Rajan Malik
Graduate Student
Electrical Engg.
University of south Florida


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
MEMS Technology Review
Mentor Graphics Corporation