MEMSnet Home: MEMS-Talk: Help! I could not remove S1818 on top of my design layer
Necessity of HCl dip after PZT etch
2004-01-05
Robert D White
Help! I could not remove S1818 on top of my design layer
2004-01-06
sokwon Paik
Help! I could not remove S1818 on top of my design layer
2004-01-07
Tony Li
Help! I could not remove S1818 on top of my design layer
2004-01-07
Mighty Platypus
Help! I could not remove S1818 on top of my design layer
Mighty Platypus
2004-01-07
I've used Baker ALEG-355 (heated to 70C) as a solvent for removing
stubborn PR. It typically doesn't attack metals. Perhaps that will work.

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Facts are stubborn, but statistics are more pliable."
   -- Mark Twain

On Mon, 5 Jan 2004, sokwon Paik wrote:

>
> I tried to remove s1818 layer after I deposited my
> designed layer. I used MF319 as I did always but it
> didn't removed s1818 layer clearly. I tried to use
> acetone to remove this s1818 layer but it failed.
> some remained s1818 layer covered my design layer.
> I tried to use shipley 1165 remover but it failed.
> I'm thinking of using RIE. But I'm afraid it could
> hurt the seed layer also.
>
> Anybody have any idea of removing this layer?
>
> If you let me know it then it would be very great.
>
> Thanks,
>
> Sokwon Paik
> Ph.D student
> Texas A&M University
>
> __________________________________
> Do you Yahoo!?
> Yahoo! Hotjobs: Enter the "Signing Bonus" Sweepstakes
> http://hotjobs.sweepstakes.yahoo.com/signingbonus
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing