MEMSnet Home: MEMS-Talk: seeing glass alignment keys
seeing glass alignment keys
2004-01-08
ERIC SIMONE
2004-01-09
David Nemeth
2004-01-09
Vic Kley
2004-01-09
[email protected]
seeing glass alignment keys
ERIC SIMONE
2004-01-08
Hello,

An interesting problem has arisen and I was wondering if anyone had any
suggestions. I'm processing on glass chips and the first step is a glass etch.
However, this means that my first set of alignment marks are transparent and I'm
having a hard time finding them with the aligner to line up the next mask. I've
tried darkening them in with a marker but that doesn't seem to help. Any ideas?
Thanks much.

-Eric





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Tanner EDA by Mentor Graphics
University Wafer