Etchants/etch rates for W and NiSi
Customer Service
2004-01-13
Transene Company manufactures Tungsten Etchant TFW.  TFW etches W at a rate
of approximately 130 angstroms/second at 30 deg C.  TFW will not attack
SiO2.

Please visit Transene's website, www.transene.com, for technical literature.
I am available if you have additional questions.

Regards,

Christopher Christuk
Transene Company
Tel:  978 777 7860
email:  [email protected]
>
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
MEMS Technology Review
Mentor Graphics Corporation