Re: Polyimide info wanted
1995-09-21
Shekhar Bhansali
1995-09-22
Gang Lin
1995-09-22
Dr. Kevin Walsh
1995-09-23
Bill Lapson
1995-09-26
Dr. Kevin Walsh
Re: Polyimide info wanted
Dr. Kevin Walsh
1995-09-22
I'm not familiar with PIX L110, but I just got some polyimide from some other
places. OCG makes a polyimide, DuPont makes a polyimide they call Pyralan(I'm
not sure of the spelling and I cannot check on it because I am at my home), and
Amoco makes a series called Ultradel.

If you need tel no, let me know

Kevin Walsh
--
Dr. Kevin M. Walsh
Electrical Engineering Department, Speed Scientific School
University of Louisville, Louisville, KY 40292
(502) 852-0826
Internet address: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Addison Engineering