MEMSnet Home: MEMS-Talk: wet oxidation of silicon
wet oxidation of silicon
2004-01-19
Isa Kiyat
the gap between substrates of wafer-bonding
2004-01-20
Chieh Jayne Woo
wet oxidation of silicon
Isa Kiyat
2004-01-19
I will try to oxidize silicon. I have found some flow rates about 1 to 2
Liters/min in some references while 0.1 Liters/min in some other for N2.
Which one sounds reasonable? comments please.
=================================

Isa Kiyat




reply