MEMSnet Home: MEMS-Talk: 1X 7 inch Mask Cleaning
1X 7 inch Mask Cleaning
2004-01-20
Purnendu Bikash Sahoo
2004-01-20
Mara Capovani
2004-01-20
[email protected]
1X 7 inch Mask Cleaning
Mara Capovani
2004-01-20
Hello P B Sahoo,

If you are unable to clean your masks and need to purchase a mask
cleaning system our company, Capovani Brothers Inc., has a few
Steag-Hamatech units that might fit your needs.  I have provided the
links to these items below.
Feel free to contact us if you have any questions or need more
information.


Kind regards,
Mara Capovani

Capovani Brothers Inc.
Equipment for Science and Industry
www.capovani.com
Phone: 518-346-8347
Fax: 518-381-9578

http://www.capovani.com/dp/cat/107/63160/iinfo.cfm?LCl=77423&SKU=&TVTID=
0&q=2&ItemNo=4711

http://www.capovani.com/dp/cat/107/63160/iinfo.cfm?LCl=77423&SKU=&TVTID=
0&q=2&ItemNo=4712

http://www.capovani.com/dp/cat/107/63160/iinfo.cfm?LCl=77423&SKU=&TVTID=
0&q=1&ItemNo=8738




-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Purnendu Bikash Sahoo
Sent: Monday, January 19, 2004 11:24 PM
To: [email protected]
Subject: [mems-talk] 1X 7 inch Mask Cleaning


We have 7 inch 1X mask of quartz and crome on it. We dont have any mask
cleaning system. We have tried to celan with acetone in room temp but
result was not so good.

Can you suggest typical mask cleaning procedure.


P B Sahoo



|%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%|
    |
|
    |  PURNENDU BIKASH SAHOO
|
    |
|
    |  Sr. Engineer (VLSI:Fab.)         Email : [email protected]
|
    |
|
    |  Semiconductor Complex Ltd.       Phone : 0172-2237401(off),
|
    |  Sector 72, S.A.S Nagar-160071    Mobile: 09815704433
|
    |  (Near Chandigarh) Punjub
|
    |  www.sclindia.com
|

|%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%%|




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.
Tanner EDA by Mentor Graphics