Polymide Adhesion Problem
1997-01-09
Piu Francis Man
Polymide Adhesion Problem
Piu Francis Man
1997-01-09
Dear Colleagues

        I have an adhesion problem of a think polyimide called PROBIMIDE 7020.
This polyimide supposes to have an adhesion promotor included. But I
could not get the polymide stick well to silicon or silicon oxide
substrate. Has anyone encounter the problem?

============================================================
Francis Piu Man
The University of Michigan, Ann Arbor