A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re:PDMS (Sylgard184) filler
Re:PDMS (Sylgard184) filler
2004-01-27
DARREN S GRAY
Re:PDMS (Sylgard184) filler
DARREN S GRAY
2004-01-27
Dear Greg,

By microscopic observation, the filler particles in Sylgard 184 seem to
be 1-20 microns in size, with an average size of approximately 10 microns.
You can have a look yourself by placing liquid pdms on glass and
spinning on a spin coater until the particles emerge from the fluid.

-Darren

Darren Gray
Graduate Student
Biomedical Engineering
Johns Hopkins University
Baltimore, MD, USA

> ------------------------------
>
> Message: 7
> Date: Mon, 26 Jan 2004 14:53:37 -0500
> From: Greg Randall 
> Subject: [mems-talk] PDMS (Sylgard184) filler
> To: [email protected]
> Message-ID: 
> Content-Type: text/plain; charset="us-ascii" ; format="flowed"
>
> Does anyone know what size range the filler (silica?) is for Sylgard
> 184 PDMS (or related)?
>
>
>
> ------------------------------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMS Technology Review