Hunter, Luke L
2004-02-02
Karl Cazzini
2004-02-02
Narayanan Unni
2004-02-02
William Lanford-Crick
2004-02-03
Michael D Martin
2004-02-03
Greg Miller
2004-02-03
Gary
2004-02-04
Michael L
2004-02-04
Hunter, Luke L
Quickly dissolving thick PMMA
Narayanan Unni
2004-02-02
Toluene is a very good solvent for PMMA
> I know that acetone works for dissolving PMMA but is
> there something that
> will work much faster, maybe 10 times?  PMMA
> thickness is between 300
> microns and 1500 microns.  Currently it takes 3 days
> to dissolve 1500 micron
> thick PMMA in acetone.
>
> Thanks
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/
>
>
>


=====
.......................................................
Dr.K.N.Narayanan Unni
Post Doctoral Research Associate
Laboratoire des Proprietés Optiques des Matériaux et Applications
UMR CNRS 6136, Université Angers, 2 Bd. Lavoisier, 49045
Angers Cedex, France
Ph:(33)(0)2 41735364, Fax:(33)(0)2 41735216

__________________________________
Do you Yahoo!?
Yahoo! SiteBuilder - Free web site building tool. Try it!
http://webhosting.yahoo.com/ps/sb/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group