A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Quickly dissolving thick PMMA
Quickly dissolving thick PMMA
2004-02-02
Hunter, Luke L
2004-02-02
Karl Cazzini
2004-02-02
Narayanan Unni
2004-02-02
William Lanford-Crick
2004-02-03
Michael D Martin
2004-02-03
Greg Miller
2004-02-03
Gary
2004-02-04
Michael L
2004-02-04
Hunter, Luke L
Quickly dissolving thick PMMA
Gary
2004-02-03
You could also try mesitylene from JT Baker. Gary

-----Original Message-----
From:   Greg Miller [SMTP:[email protected]]
Sent:   Tuesday, February 03, 2004 10:18 AM
To:     General MEMS discussion
Subject:        RE: [mems-talk] Quickly dissolving thick PMMA

Try 1165 or pure NMP heated to 80 C

Greg

-----Original Message-----
From: Hunter, Luke L [mailto:[email protected]]
Sent: Monday, February 02, 2004 1:45 PM
To: '[email protected]'
Subject: [mems-talk] Quickly dissolving thick PMMA


MEMS folk,

I know that acetone works for dissolving PMMA but is there something that
will work much faster, maybe 10 times?  PMMA thickness is between 300
microns and 1500 microns.  Currently it takes 3 days to dissolve 1500 micron
thick PMMA in acetone.

Thanks
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering