MEMSnet Home: MEMS-Talk: What could be wafer surface temperature
What could be wafer surface temperature
2004-02-08
MT Klaus Beschorner
2004-02-09
Gary
What could be wafer surface temperature
MT Klaus Beschorner
2004-02-08
 >   10. What could be wafer surface temperature during sputter
 >       deposition w/ Al deposition, 10000W, 150sccm Ar flow,  12min
 >       deposition time? (Cheol Han)

The wafer surface is where vapour phase Al condenses to the solid state,
so as an estimate you can use the boiling point of Al.

If what you really mean is the substrate temperature, without active heat
sinking (backside gas), a 2µm Al deposition in 1.5 min. has been measured
to heat a standard wafer from room temp. to over 550 C.

best regards,
klaus

--
Klaus Beschorner
Metron Technology Europe, PVD (Eclipse) Process Manager
Drosselweg 6,71120 Grafenau,Germany. Tel +49-7033-45683




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation