SU8 Information
2004-02-11
Brubaker Chad
SU8 Information
Brubaker Chad
2004-02-11
Christian,

A good place to start is the following web site:

http://aveclafaux.freeservers.com/SU-8.html


Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   [email protected] [mailto:mems-talk-
[email protected]]  On Behalf Of [email protected]
Sent:   Monday, February 09, 2004 9:23 PM
To:     General MEMS discussion
Subject:        [mems-talk] SU8 Information

Hello Lists,

I was just wondering if anyone can help me with some info on SU8.

What type of chemical is SU8, I know its an epoxy based resin but does it belong
to a
specific chemical type i.e. polyamide

Does anyone have or can lead me to the  complete reaction of SU8 from when the
radicals are formed after exposure to the crosslinking of the Epoxy groups.

Any help would be greatly appreciated.  Thank you in advance.

Best Regards,

Christian Antonio
Research Student
Industrial Research Institute Swinburne,
Melbourne,
Australia.__________________________________________________________

Christian Antonio

Industrial Research Institute Swinburne (IRIS)
533-545 Burwood Road,
Hawthorn, VIC., Australia 3122.
Tel :  +61 3  9214 5698
Fax : +61 3  9214 5050


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
The Branford Group
Tanner EDA by Mentor Graphics