MEMSnet Home: MEMS-Talk: Conductive substrates for processing SU-8
Conductive substrates for processing SU-8
2004-02-11
Mark Leonard
2004-02-12
Edward Blackwell
2004-02-11
Michael D Martin
2004-02-11
[email protected]
Conductive substrates for processing SU-8
Michael D Martin
2004-02-11
Perhaps you could use a heavilly doped wafer.

-Mike Martin

>>> [email protected] 2/11/2004 5:58:36 AM >>>
Hello all,

I am currently using the UV-LIGA process with SU-8 to fabricate
metallic MEMS devices as part of my PhD work. Since my devices are
removed from the substrate after fabrication I use the cheapest wafers
possible, onto which I deposit a conductive seed layer by chemical
vapour deposition to form a plating base. I was wondering if anyone has
experience using a suitable conductive substrate which cuts out the need
to deposit the conductive seed layer and hence save on processing time.
I have noticed that SU-8 does not adhere well to some surfaces such as
copper. I have also noticed that substrates which do not have a mirror
finish result in poor quality features, presumably because of
scattering. It would be much appreciated if anyone has any suggestions
on potential conductive substrates that I can try for my process.


Mark
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Mentor Graphics Corporation
Nano-Master, Inc.