Does anyone know of a deep (10 t0 50 *m deep) process for anisotropic
etching of quartz wafers?  Do any of the deep RIE's work?
 Dan Ehrlich, Rm 341 MIT/Whitehead Institute of Biomedical Research,
Cambridge MA.