MEMSnet Home: MEMS-Talk: Does concentrated HF etch Au
Does concentrated HF etch Au
2004-02-16
li Yu
2004-02-16
David Nemeth
2004-02-16
Jing Liu
2004-02-16
Tres Brooks
2004-02-16
[email protected]
Does concentrated HF etch Au
David Nemeth
2004-02-16
HF does not etch gold, but it might etch the adhesion layer or underlying
substrate, causing it to peel off.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
-----Original Message-----
From: [email protected]
[mailto:[email protected]]On
Behalf Of li Yu
Sent: Sunday, February 15, 2004 9:14 PM
To: [email protected]
Subject: [mems-talk] Does concentrated HF etch Au


I want to put a wafer with 2000A Au in 49% HF for 30 minute, Is that Ok?
Thanks in advance.
 Lili


---------------------------------
Do you Yahoo!?
Yahoo! Finance: Get your refund fast by filing online
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing