Hi,

I have achieved a 45 microns/hour Si etch rate with TMAH (thank's to all your
answers).

In order to keep an etch rate over 30 microns/hour, when should I do another
TMAH solution?

I would also like to know if the TMAH attacks Nickel?

Thank's


Guy Haché, M.Sc.A.
Assistant de recherche, research assistant
--------------------------------------------------------
Département de génie électrique et de génie informatique
Université de Sherbrooke
2500, boulevard Université
Sherbrooke (Québec) Canada
J1K 2R1
Téléphone/phone : (819) 821-8000 3706
Télécopieur/fax : (819) 821-7937
e-mail: [email protected]
--------------------------------------------------------

--------------------------------------------------------------------------------





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing