Hi Guy,

I think your time of the etch process is important when considering the
effect of TMAH on Nickel. TMAH definitely etches nickel when etched over a
period of time ( say for more than a  couple of hours).Even for a shorter
time, TMAH would cause considerable surface roughness. It all depends on
what you are using the nickel layer for.
Sreeram


> Hi,
>
> I have achieved a 45 microns/hour Si etch rate with TMAH (thank's to all
your
> answers).
>
> In order to keep an etch rate over 30 microns/hour, when should I do
another
> TMAH solution?
>
> I would also like to know if the TMAH attacks Nickel?
>
> Thank's
>
>
> Guy Haché, M.Sc.A.
> Assistant de recherche, research assistant
> --------------------------------------------------------
> Département de génie électrique et de génie informatique
> Université de Sherbrooke
> 2500, boulevard Université
> Sherbrooke (Québec) Canada
> J1K 2R1
> Téléphone/phone : (819) 821-8000 3706
> Télécopieur/fax : (819) 821-7937
> e-mail: [email protected]

----------------------------------------------------------------------------
----------------- CONFIDENTIAL AND PRIVILEGED INFORMATION ------------------

This email, including attachments, contains information that is privileged,
confidential or subject to non-disclosure agreements or intellectual
property laws.  This email, including attachments, constitutes non-public
information intended to be conveyed only to the designated recipient(s).  If
you are not the intended recipient, please delete this email, including
attachments, and notify the sender by return mail, email, or by calling (ALL
CONTACT INFORMATION LISTED BELOW). The unauthorized review, use,
dissemination, distribution, or reproduction of this email, including
attachments, is prohibited and may be unlawful.

APPLIED IMAGE Group / Optics subsidiary
4400 South Santa Rita Avenue
Tucson, AZ 85704
phone:  520-806-3800
fax:    520-806-3899

----------------- CONFIDENTIAL AND PRIVILEGED INFORMATION ------------------
----------------------------------------------------------------------------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
Addison Engineering