MEMSnet Home: MEMS-Talk: How to remove carbon from Ta film
How to remove carbon from Ta film
2004-02-21
Suhua Jiang
How to remove carbon from Ta film
Suhua Jiang
2004-02-21
Hi all,
I implanted C in Ta, but some C deposite on Ta, thickness is not constant
for different dose......
Is there any method to remove C from Ta, and also won't let implanted C come
out.
Thanks a lot

National Microanalysis Center
Materials Science Department
Fudan University
220# Handan Road
Shanghai, 200433
China
Tel: 86-21-65642380

_________________________________________________________________
Add photos to your e-mail with MSN 8. Get 2 months FREE*.
http://join.msn.com/?page=features/featuredemail



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics