MEMSnet Home: MEMS-Talk: adhesion of oxide to evaprated chromium
adhesion of oxide to evaprated chromium
2004-02-21
Anna Ohlander
2004-02-23
JOHNSON,MARK (HP-Corvallis,ex1)
adhesion of oxide to evaprated chromium
JOHNSON,MARK (HP-Corvallis,ex1)
2004-02-23
Anna,

I think you will find that chromium does form an oxide.  There are several
references in the literature related to this, since it is used as a coating
metal for SEM.

Mark

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of
Anna Ohlander
Sent: Saturday, February 21, 2004 10:26 AM
To: [email protected]
Subject: [mems-talk] adhesion of oxide to evaprated chromium


Hello,

Does anybody know anything about the adhesion of PECVD si oxide to
evaporated chromium? I've read that Chromium doesn't form a native oxide in
room temperature. What's the secret behind it's potential as an adhesion
layer?

/ Anna

_________________________________________________________________
Hitta rätt på nätet med MSN Sök http://search.msn.se/


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.
MEMS Technology Review