Mask for concentrated HF
Matthieu Gaudet
2004-02-26
Generally, I use AZ1518 photoresist (2 microns) to etch 400nm of SiO2.
at the end of the process (about 6 min ) the photoresist is still there and
doesn't seems to be attacked by HF 50%.

I hope it will help you

Matthieu
----- Original Message -----
From: "Brent Garber" 
To: "General MEMS discussion" 
Sent: Tuesday, February 24, 2004 4:30 PM
Subject: Re: [mems-talk] Mask for concentrated HF


> Hiroaki,
>
> I have always used sputtered Cr/Au.  Depending on glass thickness will
> determine if you will get much or any under cutting.
>
> Brent
>
> Hiroaki SUZUKI wrote:
>
> > Hi all
> >
> > Please allow me to ask one simple question. it might be in the past
> > discussion...
> > What is the best mask material for the glass etching with concentrated
HF?
> >
> > Hiroaki
> >
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.memsnet.org/
>


----------------------------------------------------------------------------
----


> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing