2004-02-26
Aamer Mahmood
2004-02-27
Neal Ricks
2004-02-27
Tripp, Marie Kathleen
2004-02-27
Greg Miller
Aluminum Oxide etchant
Aamer Mahmood
2004-02-26
Hello everyone,This is my first post to the group.
I have searched this topic in the archives but haven't found a spot on
answer.
I need to sputter Aluminum Oxide on top of Spin on Glass and then
pattern and etch the Oxide.
What etchants can I use for the Aluminum Oxide etch?
Any particular masking materials or just the photoresist would do?
How does Aluminum Oxide react to CF4 (SOG etchant)?
Conversely, how does SOG react to the Aluminum Oxide etchant?
Any info on the selectivity of the etchants would also be helpful.
Regards.

Aamer Mahmood
Graduate Assistant
Microsensors lab
Department of Electrical Engineering
University of Texas at Arlington
Arlington TX 76019
email: [email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation