RIE of sub-micron Si structures
2004-02-26
Josef Kouba
2004-02-27
Burkhard Volland
2004-03-01
[email protected]
RIE of sub-micron Si structures
[email protected]
2004-03-01
Hi,

The Plasmalab 80Plus has been used for a range of sub-micron structures,
including diffraction gratings and photonic crystals, so should be capable
of achieving your 200x200nm holes.  You do not mention the type of mask you
are using for this.  If you have PMMA (e-beam written) you should be aware
that this has less plasma resistance than conventional Novolak resists, so
could cause problems. You may need to reduce the amount of oxygen if the
resist is going too fast.

Regarding the comment on Chlorine - we would not recommend using chlorine in
an open load system such as the Plasmalab80Plus, unless you were using a
nitrogen glove-box on it.

Martin (Oxford Instruments Plasma Technology)

 ###  OXFORD INSTRUMENTS   http://www.oxford-instruments.com/  ###

Unless stated above to be non-confidential, this E-mail and any
attachments are private and confidential and are for the addressee
only and may not be used, copied or disclosed save to the addressee.
If you have received this E-mail in error please notify us upon receipt
and delete it from your records. Internet communications are not secure
and Oxford Instruments is not responsible for their abuse by third
parties nor for any alteration or corruption in transmission.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.