jo ed
2004-03-02
Mighty Platypus
2004-03-02
ROSTAING Cedric 177671
2004-03-03
William Lanford-Crick
oxide wet etch on ito
jo ed
2004-03-02
Hello

I have a substrate coated with ito followed by oxide.
Does anyone know of a selective wet etch process to
remove the oxide put keep the ito?

cheers,
Jo

__________________________________
Do you Yahoo!?
Yahoo! Search - Find what you’re looking for faster
http://search.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review