Jin Jiandong,

Gold bonding can indeed be used for a strong wafer-level bond. A lot of good
information on this process has come out of MIT.  One paper is "Wafer-Level
Thermocompression Bonds" by Tsau, Schmidt, and Spearing at MIT, from Advanced
Materials for Micro- and Nano-Systems (AMMNS), Jan 2003. Wafer preparation,
process, and equipment are discussed.

Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   [email protected] [mailto:mems-talk-
[email protected]]  On Behalf Of jane jin
Sent:   Tuesday, March 02, 2004 12:57 AM
To:     [email protected]
Subject:        [mems-talk] Au-Au bonding

Hello, list members
I am trying to bond three wafers together, and want to know if Au-Au can be
boned tightly, if it works , what is the principle, and in what condition it
will be bonded.
Thanks for any related answers.

Jin, Jiandong




---------------------------------
Do you Yahoo!?
Yahoo! Search - Find what you're looking for faster.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
University Wafer
MEMS Technology Review